We are among the eminent manufacturers, suppliers, wholesalers and traders of LR Grade AH36 Shipbuilding Steel Plates in the industry as per the various national as well as international standard and specifications.
LR AH36 Chemical Composition:
| Grade | The Element Max (%) | ||||||
| C | Si | Mn | P | S | Al | N | |
| LR AH36 | 0.18 | 0.05 | 0.9-1.6 | 0.035 | 0.035 | 0.015 | |
| Nb | V | Ti | Cu | Cr | Ni | Mo | |
| 0.02-0.05 | 0.03-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 | |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
LR Grade AH36 Mechanical property:
| Grade |
| Mechanical Property | Charpy V Impact Test | ||||
| Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
| LR AH36 | mm | Min Mpa | Mpa | Min % | 0 | J | J |
| t≤50 | 355 | 490-630 | 21% | 24 | 34 | ||
| 50<t≤70 | 355 | 490-630 | 21% | 27 | 41 | ||
| 70<t≤100 | 355 | 490-630 | 21% | 34 | 50 | ||
| Note: Energy 1 is transverse impact test, Energy 2 is longitudinal | |||||||
LR AH36 Shipbuilding steel plates are mainly used for making the offshore oil drilling platform, the hull of ship building and ship repairing, the platform pipe joints and other components.
LR Grade AH36 Tests:
LR Grade AH36 (LR/AH36) steel plate contains Tensile Tests and Impact Tests. The UT (Ultrasonic Testing), the third party test, Z15, Z25, Z35 test and other tests are also available as customers' requirement.
| Equivalent steel grade of LR/AH36 | |||||||
| DNV | GL | ABS | BV | CCS | NK | KR | RINA |
| NV A36 | GL-A36 | AB/AH36 | BV/AH36 | CCS/A36 | K A36 | R A36 | RI/A36 |

Address:Zhengzhou city in China.
Phone:0086-371-86151827
Email:



Address: Zhengzhou city in China.